ASTM A312 TP310 SCH 40 zanglamaydigan po'latdan yasalgan dumaloq quvur
Xabar QOLDIRISH
Agar siz 1000 darajadan yuqori haroratlarda, oksidlovchi atmosferalarda va termal aylanish sharoitida uzoq muddatli barqaror ishlashga qodir bo'lgan sanoat quvurlarini qidirsangiz, ASTM A312 TP310 dumaloq quvur304, 316L yoki hatto 309S dan ko'ra ishonchliroq tanlovdir.
ASTM A312 TP310 zanglamaydigan po'lat quvur yetkazib beruvchi, ishlab chiqaruvchi
GNEE ikkalasini ham ta'minlaydiASTM A312 TP310/310S choksiz va payvandlangan quvurlar, tashqi diametrlari (OD) 6 mm dan 610 mm gacha va devor qalinligi SCH 5S dan XXS gacha bo'lgan to'liq seriyani qo'llab-quvvatlaydi. Mahsulotlar standart ravishda eritma-tavlangan va tuzlangan holatda yetkazib beriladi, so‘rov bo‘yicha moslashtirilgan sirt ishlovlari, jumladan, yorqin yumshatish, ichki/tashqi parlatish va qumtoshlash mumkin. Barcha mahsulotlar EN 10204 3.1/3.2 material sertifikatlari va SGS, BV yoki TÜV-uchunchi tomon tekshiruvlari bilan ta'minlanishi mumkin.

Biz yetkazib beradigan TP310 zanglamaydigan po‘lat quvurlari yuqori{1}}xromli-nikel ostenitik issiqlik-bardoshli po‘latdan yasalgan bo‘lib, tarkibida 24,0-26,0% xrom va 19,0-22,0% nikel mavjud. Uning doimiy xizmat qiluvchi antioksidant harorati 1035 darajagacha, qisqa muddatli-1150 darajagacha haroratga chidamlilik bilan ishlaydi. Yuqori haroratlarda u zich va barqaror himoya oksidi qatlamini hosil qiladi, u yuqori{15}}haroratning shkalasi, karbürizatsiyasi va oltingugurtga-tug'in gazining termal korroziyasiga samarali qarshilik ko'rsatadi. Bundan tashqari, uning valentlik kuchi 600 daraja haroratda ham taxminan 400 MPa boʻlib qoladi, bu esa uni sanoat pechlari, issiqlik bilan ishlov berish liniyalari va yuqori haroratli quvurlar uchun ideal qiladi.

ASTM A312 TP310 zanglamaydigan po'lat quvur

ASTM A312 TP310S SS SMLS trubkasi

ASTM A312 TP310 zanglamaydigan po'latdan yasalgan BA trubkasi
TP310 va TP310S: qanday tanlash kerak?
Ish sharoitlari payvandlangan tuzilmalar, 650–900 daraja sezgirlik harorati oralig'ida uzoq muddatli ishlash yoki donalararo korroziyaga chidamlilik talablari, TP310S zanglamaydigan po'lat quvur bilan bog'liq bo'lsa.juda tavsiya etiladi. Past{1}}uglerodli modifikatsiyalangan nav sifatida 310S uglerod miqdorini 0,08% dan kam yoki unga teng darajada nazorat qiladi, bu esa payvandlash va uzoq{4}}yuqori{5}}{5}}haroratli xizmat paytida karbid yog‘inlarining tushishi xavfini sezilarli darajada kamaytiradi. Bu issiqlik almashtirgichlar, chiqindi gazni tozalash uskunalari, yoqish pechlari va yuqori{7}}haroratli quvurlar tizimlari uchun juda mos keladi, bu esa keng qamrovli payvandlashni talab qiladi.
ASTM A312 TP310/310S quvur Kimyoviy tarkibi
| Baho | UNS | C (maksimal) | Mn (maksimal) | P (maksimal) | S (maksimal) | Si (maksimal) | Cr | Ni |
| TP310 | S31000 | 0.15% | 2.00% | 0.045% | 0.030% | 1.00% | 24.0 – 26.0% | 19.0 – 22.0% |
| TP310S | S31008 | 0.08% | 2.00% | 0.045% | 0.030% | 1.00% | 24.0 – 26.0% | 19.0 – 22.0% |
ASTM A312 TP310/310S choksiz quvur mexanik xususiyatlari
| Baho | Kuchlanish kuchi, min | Hosildorlik kuchi (0,2% ofset), min | 2 dyuym yoki 50 mm gacha cho'zilish, min | Qattiqlik (Brinell) maks | Qattiqlik (Rokvell B) maks |
| TP310 | 515 MPa (75 ksi) | 205 MPa (30 ksi) | 35% | 192 HBW | 90 HRB |
| TP310S | 515 MPa (75 ksi) | 205 MPa (30 ksi) | 35% | 192 HBW | 90 HRB |
ASTM A312 o'lchovli toleranslar
| Standart | Tashqi diametrning bardoshliligi (mm) | Qalinligi tolerantligi | Uzunlik bardoshlik (mm) | |||
| ASTM A312 |
[10.29~48.26] | +0.4/-0.8 | 10.3~73 | +20% / -12.5% | +6/-0 | |
| 88,9~457 T/D 5% dan kam yoki unga teng | +22.5%/-12.5% | |||||
| (48.26~114.30] | ±0.80 | 88.9~457 T/D>5% | +15%/-12.5% | |||
| (114.30~219.08] | +1.6/-0.8 | 508 T/D dan yuqori<5% | +22.5%/-12.5% | |||
| (219.08~457.20] | +2.4/-0.8 | 508above T/D>5% | +15%/-12.5% | |||
ASTM A312 TP310/310S quvurining og'irligi
Eslatma: Nazariy og'irlik zichligi yordamida hisoblanadi7,98 g/sm³ (0,288 lb/in³)310-sinfdagi nikel va xromning yuqori miqdori tufayli.
| NPS (dyuym) | OD (dyuym) | OD (mm) | SCH 40 Vt (dyuym) | SCH 40 Vt (mm) | Og'irligi (kg/m) | Og'irligi (lb/ft) |
| 1/2" | 0.840 | 21.34 | 0.109 | 2.77 | 1.28 | 0.86 |
| 3/4" | 1.050 | 26.67 | 0.113 | 2.87 | 1.71 | 1.15 |
| 1" | 1.315 | 33.40 | 0.133 | 3.38 | 2.54 | 1.71 |
| 1-1/4" | 1.660 | 42.16 | 0.140 | 3.56 | 3.44 | 2.31 |
| 1-1/2" | 1.900 | 48.26 | 0.145 | 3.68 | 4.11 | 2.76 |
| 2" | 2.375 | 60.33 | 0.154 | 3.91 | 5.52 | 3.71 |
| 2-1/2" | 2.875 | 73.03 | 0.203 | 5.16 | 8.77 | 5.89 |
| 3" | 3.500 | 88.90 | 0.216 | 5.49 | 11.47 | 7.71 |
| 3-1/2" | 4.000 | 101.60 | 0.226 | 5.74 | 13.78 | 9.26 |
| 4" | 4.500 | 114.30 | 0.237 | 6.02 | 16.32 | 10.97 |
| 5" | 5.563 | 141.30 | 0.258 | 6.55 | 22.11 | 14.86 |
| 6" | 6.625 | 168.28 | 0.280 | 7.11 | 28.69 | 19.28 |
| 8" | 8.625 | 219.08 | 0.322 | 8.18 | 43.21 | 29.04 |
| 10" | 10.750 | 273.05 | 0.365 | 9.27 | 61.22 | 41.14 |
| 12" | 12.750 | 323.85 | 0.406 | 10.31 | 80.98 | 54.42 |
ASTM A312 TP310 dumaloq quvur HS kodi
| Mahsulot tavsifi | HS kodi | HS kodi tavsifi |
|---|---|---|
| ASTM A312 TP310 choksiz zanglamaydigan po'lat quvur | 7304.49 | Choksiz quvurlar, quvurlar va ichi bo'sh profillar, zanglamaydigan po'latdan va boshqalar |
| ASTM A312 TP310 payvandlangan zanglamaydigan po'lat quvur | 7306.40 | Zanglamaydigan po'latdan payvandlangan quvurlar, quvurlar va ichi bo'sh profillar |
ASTM A312 TP310 zanglamaydigan po'latdan yasalgan choksiz quvurlar uchun ilovalar:
Pech komponentlari (mufellar, retort, konveyer bantlari).
Issiqlik almashinuvchilari va qozon quvurlari.
Radiatsion quvurlar va bug 'qozonlari.
Neft-kimyoni qayta ishlash uskunalari.
Kriogen komponentlar
Agar siz xarid yoki loyihani rejalashtirmoqchi bo'lsangiz, menga ayting: Sizga qanday nominal quvur o'lchami (NB/OD) va uzunligi kerak? Choksiz yoki payvandlangan quvurni afzal ko'rasizmi? Men sizga aniq mavjudligi yoki texnik ma'lumotlarini topishda yordam bera olaman.
TP310 zanglamaydigan po'lat quvur narxi kg uchun
310 dona zanglamaydigan po'lat quvurning ulgurji narxi har bir kilogramm uchun 2,20 dan 4,10 dollargacha (taxminan $ 1,180 dan 4,100 dollargacha) o'zgarib turadi, mahalliy chakana yoki ichki sanoat bozorlarida narxlar odatda kilogramm uchun taxminan 3,50 dan 11,00 dollargacha, qayta ishlash darajasiga qarab.
Sifat nazorati
TP310 tez-tez xavfli yuqori{1}}harorat va yuqori-bosimli ilovalarda qo'llanilganligi sababli, jo'natishdan oldin quyidagi sinovlar o'tkaziladi:
PMI (Positive Material Identification) tahlili
Gidrostatik sinov: Har bir quvur bosim sinovidan o'tadi.
Eddy Current yoki Ultrasonik Sinov (UT): Quvur devorida teshiklar, yoriqlar yoki shlak qo'shimchalari yo'qligiga ishonch hosil qilish uchun, odatda, 100% buzilmaydigan sinov- talab qilinadi.
Radiografik sinov (RT): Payvandlangan quvurlar uchun payvand chokini rentgen nurlari bilan tekshirish muhim ahamiyatga ega.




Yuqori-Sifatli qadoqlash
Oxirgi himoya: changning ichki devorlarga kirishiga yo'l qo'ymaslik uchun-ikki uchiga yuqori quvvatli plastik qopqoqlar o'rnatilgan va uchlarini zarbadan-deformatsiyadan himoya qiladi.
Yuzaki o'rash:
Yorqin tavlangan (BA) quvurlar: alohida-alohida plastik qoplarga solinadi, keyin qatlamlarga o'raladi.
Tuzlangan (AP) quvurlar: suv o'tkazmaydigan to'qilgan mato yoki VCI{0}}zangga qarshi plyonkaga to'liq o'ralgan.
Kuchaytirilgan yog'och qutilar: GNEE issiqlik almashtirgich quvurlari uchun fumigatsiyasiz{0}}kontrplak qutilaridan foydalanishni buyuradi (ISPM-15 xalqaro eksport standartlariga mos).


TSS
TP310 suyuq azot kabi kriyojenik muhitda ishlatilishi mumkinmi?
Ha. TP310 zanglamaydigan po'lat ostenitik tuzilishga ega bo'lib, juda past haroratlarda (kriogen sharoitlarda) ham mukammal mustahkamlik va juda past magnit o'tkazuvchanlikni ta'minlaydi. Uning past -harorat ko‘rsatkichlari aslida 304-sinfdan ustundir.
TP310 SCH 40 quvurini payvandlash qiyinmi?
TP310 yaxshi payvandlanish qobiliyatiga ega, ammo yuqori qotishma tarkibi tufayli quyidagi fikrlarga e'tibor berish kerak:
Issiq yorilish xavfi: payvand choklari issiq yorilishga moyil, shuning uchun o'tish oralig'idagi haroratni qat'iy nazorat qilish kerak.
Tavsiya etilgan payvandlash materiallari: Mos keladigan ER310 payvandlash paychalarining yoki E310 payvandlash elektrodlaridan foydalaning.
Nima uchun TP310 304 dan qimmatroq?
Bu, birinchi navbatda, juda yuqori nikel (Ni) va xrom (Cr) tarkibiga bog'liq. 304-navda taxminan 8% nikel mavjud, 310-da esa 19-22% (304-dan deyarli 2,5 baravar ko'p). Nikel va xrom qimmatbaho metallar bo'lib, xom ashyo xarajatlarini bevosita belgilaydi.